一、代表性的論文:
1. Bin Xu, Mu-sen Li, Li Li, Ai-min Xu and Yu-chao Niu. A relation between a metallic film covering on diamond and diamond nucleation and growth at high-temperature–high-pressure in a Ni–Mn–C system, Materials Science and Engineering A, 2007, 454-455: 293~299
2. Bin Xu, Mu-sen Li, Jian-jun Cui, Jian-hong Gong and Shu-hua Wang. An investigation of a thin metal film covering on HPHT as-grown diamond from Fe-Ni-C system, Materials Science and Engineering A, 2005, 396: 352~359
3. XU Bin, LI Musen, YIN Longwei, CUI Jianjun, LIU Yuxian, GONG Jianhong. Microstructures of metallic film and diamond growth from Fe-Ni-C system, Chinese Science Bulletin, 2002, 47 (15): 1258~1262
4. XU Bin, LI Mu-Sen, YIN Long-Wei, CUI Jian-Jun, GONG Jian-Hong. Effect of Metallic Film in Diamond Growth from a Fe-Ni-C System at High Temperature and High Pressure, Chinese Physics Letters, 2003, 20 (5): 759~762
5. XU Bin, CUI Jian-Jun, LI Mu-sen, LI Cheng-mei, CHU Fu-min, FENG Li-ming. Carbide Identification in Different Regions of a Thin Metal Film Covering on HPHT As-Grown Diamond Single Crystal from Ni-Mn-C System, Chinese Physics Letters, 2005, 22 (2): 478~481
6. Bin XU, Musen LI, Longwei YIN, Jianjun CUI, Jianhong GONG. AFM Study on Interface of HTHP As-grown Diamond Single Crystal and Metallic Film, Journal of Materials Science & Technology, 2003, 19 (2): 113~116
7. XU Bin, LI Mu-sen, YIN Long-wei, Liu Yu-xian, CUI Jian-jun, GONG Jian-hong. Interface between metallic film from Fe-Ni-C System and HPHT as–grown diamond single crystal, Transaction of Nonferrous Metals Society of China, 2003, 13 (4): 902~906
8. Bin XU, Shuhua Wang, Yupeng Lu, Jianjun Cui and Musen Li. Effect of Micro-addition Rare Earth and Chrome on Friction and wear Behavior of boronized layer. Key Engineering Materials, 2005, 297-300: 1401~1405
9. 許斌,宮建紅,李木森,崔建軍,許愛民,高洪吉. 鐵基金屬包膜內(nèi)的Fe3C行為與高溫高壓金剛石單晶生長, 金屬學報, 2005, 41 (10): 1101~1105
10. 許斌,李木森,宮建紅,章亞明,牛玉超,景財年. 鐵基金屬包膜的Mössbauer參量及其在金剛石合成中的催化作用, 金屬學報, 2004, 40 (8): 810~814
11. 許斌,崔建軍,王淑華,李木森,李成美,馮立明. 人造金剛石單晶鐵基金屬包膜的精細結(jié)構(gòu). 金屬學報, 2005, 41 (4): 444~448
12. Bin XU, Le YANG, Shibo XING and Li LI . Effect of Plastic Deformation at Room Temperature on Powder RE-chrome-boronizing for Medium Carbon Steel, Key Engineering Materials, 2007, 353-358: 575~578
13. 許斌,宮建紅,李麗,李木森,宿慶財,高洪吉. Fe3C型碳化物與人造金剛石晶面價電子結(jié)構(gòu)分析, 硅酸鹽學報, 2006, 34 (6): 656~661
14. 許斌,李木森,崔建軍,宮建紅,田清波,高洪吉. 金剛石單晶/鎳基金屬包膜界面的相結(jié)構(gòu)和形貌,硅酸鹽學報, 2006, 34 (3): 271~276
15. 許斌,李木森,李士同, 項東,牛玉超,景財年. 鐵基觸媒生長金剛石過程中金屬包膜成分研究,硅酸鹽學報, 2004, 32 (8): 936~941
16. 許斌,李木森,尹龍衛(wèi),崔建軍. 鐵基觸媒合成金剛石形成的金屬包膜的組織結(jié)構(gòu), 硅酸鹽學報, 2003, 31 (5): 470~475
17. 許斌,高洪吉,馬紅霞. 高溫高壓下石墨-Ni70Mn25Co5體系中金剛石單晶合成工藝參數(shù)對金屬包膜的影響, 人工晶體學報, 2007, 36(4): 904-907
18. 許斌,李木森,尹龍衛(wèi),崔建軍,劉玉先,宮建紅. 金屬包膜的結(jié)構(gòu)與鐵基觸媒合成金剛石的生長, 科學通報, 2002, 47 (9): 669-673
19. 許斌, 李木森. 降低滲硼層本質(zhì)脆性對其摩擦磨損特性的影響,機械工程學報, 2002, 38(11): 131~134
20. 許斌, 馮承明,楊膠溪. 碳化鎢-高鉻鑄鐵表面復合材料耐磨粒磨損性能的研究,摩擦學學報,1998,18(4): 322~326
21. 許斌, 馮承明,張業(yè)民. 鎳基碳化鎢自熔合金噴焊層與硼化物層磨損特性的對比研究,摩擦學學報,1998,18(2): 152~156
二、已授權(quán)的國家發(fā)明專利:
1.一種工件滲前冷變形的硼-鉻-稀土共滲工藝(專利號:ZL 2006 1 0045187.2)
2.一種合成高強度金剛石用粉末冶金觸媒(專利號:ZL 2007 1 0013220.8)