發(fā)表的主要論文 1. Deng Jianxin etal. Friction and wear behaviors of the PVD ZrN coated carbide in sliding wear tests and in machining processes. Wear, 2008, 264 (3-4): 298-307 2. Deng Jianxin etal. Effect of residual stresses on the erosion wear of laminated ceramic nozzles. Materials Characterization, 2008, 59 (1): 1-8 3. Deng Jianxin etal. Wear mechanisms of PVD ZrN coated tools in machining. International Journal of Refractory Metals & Hard Materials. 2008, 26 (3): 164-172 4. Deng Jianxin etal. Erosion wear behaviours of SiC/(W,Ti)C laminated ceramic nozzles in dry sand blasting processes. Materials Science Engineering, A, 2007, 444 (1-2): 120-129 5. Deng Jianxin etal. Wear mechanisms of gradient ceramic nozzles in abrasive air-jet machining. International Journal of Machine Tool and Manufacture. 2007, 47 (12-13): 2031-2039 6. Deng Jianxin etal. Development of gradient ceramic nozzle materials for sand blasting surface treatments. International Journal of Refractory Metals & Hard Materials, 2007, 25 (2): 130-137 7. Deng Jianxin etal. Erosion wear mechanisms of coal-water-slurry (CWS) ceramic nozzles. Materials Science Engineering, A, 2006, 417 (1-2): 1-7 8. Deng Jianxin etal. Self lubrication of sintered ceramic tools with CaF2 additions in dry cutting, International Journal of Machine Tool and Manufacture, 2006, 46 (9): 957-963 9. Deng Jianxin etal. Wear mechanisms of Al2O3/TiC/Mo/Ni ceramic wire-drawing dies. Materials Science Engineering A, 2006, 424 (1-2): 347-354 10. Deng Jianxin etal. Tribological behaviors of hot-pressed Al2O3/TiC ceramic composites with the additions of CaF2 solid lubricants. Journal of the European Ceramic Society, 2006, 26 (8): 1317-1323 11. Deng Jianxin etal. Wear of ceramic nozzles by dry sand blasting, Tribology International, 2006, 39 (3): 274-280 12. Deng Jianxin etal. Failure mechanisms of TiB2 particle and SiC whisker reinforced Al2O3 ceramic cutting tools when machining nickel-based alloys, International Journal of Machine Tool and Manufacture, 2005, 45 (12-13): 1393-1401 13. Deng Jianxin etal. Self-lubricating behaviors of Al2O3/TiB2 ceramic tools in dry high-speed machining of hardened steel, Journal of the European Ceramic Society, 2005, 25 (7): 1073-1079 14. Deng Jianxin. Erosion wear of boron carbide nozzles by abrasive air-jets. Materials Science Engineering, A. 2005, 408 (1-2): 227-233 15. Deng Jianxin, etal. Microstructure and mechanical properties of hot-pressed Al2O3/TiC ceramic composites with the additions of solid lubricants, Ceramic International, 2005, 31 (2): 249-256 16. Deng Jianxin etal. Wear behaviors of the ceramic nozzles in sand blasting treatments, Journal of the Euroepan Ceramic Society, 2003, 23 (2): 323-329 17. Deng Jianxin etal. Erosion wear of ceramic and cemented carbide nozzles in dry sand blasting process, British Ceramic Transactions, 2003, 102 (2) : 61-65 18. Deng Jianxin, Lee Taichiu. Effect of ultrasonic surface finishin g on thermal shock behaviour and the strength of EDMed ceramic composites, International Journal of Machine Tool and Manufacture, 2002, 42 (2): 245-250 19. Deng Jianxin, Lee Taichiu. Ultrasonic machining of alumina based ceramic composites, Journal of the Euroepan Ceramic Society, 2002, 22 (8): 1235-1241 20. Deng Jianxin etal. Microstructure and mechanical properties of hot-pressed B4C/(W,Ti)C ceramic composites, Ceramics International, 2002, 28 (4): 425-430 21. Lee Taichiu, Deng Jianxin. Mechanical surface treatments of EDMed ceramic composites for improved strength and reliability, Journal of the Euroepan Ceramic Society, 2002, 22 (4): 545-550 22. Deng Jianxin. Friction and wear behaviour of Al2O3/TiB2/SiCw ceramic composite at temperature up to 800℃, Ceramics International, 2001, 27 (2): 135-141 23. Deng Jianxin, Lee Taichiu. Surface integrity in electro-discharge machining, ultrasonic machining, and diamond saw cutting of ceramic composites, Ceramics International, 2000, 26 (8): 825-830 24. Deng Jianxin, Lee Taichiu. Techniques for improved surface integrity and reliability of machined ceramic composites, Surface Engineering, 2000, 16 (5): 411-414 25. Deng Jianxin. Effect of residual stress on the high temperature toughening behaviours of TiB2/SiCw composites, Journal of Materials Processing Technology, 2000, 98 (3):292-298 26. Deng Jianxin etal. Microstructure and mechanical properties of hot-pressed TiB2/SiCw composite. Materials Research Bulletin, 1998, 33 (4): 575-582 27. Deng Jianxin etal. Wear behaviour and mechanisms of alumina based ceramic tools in machining of ferrous and non-ferrous alloys. Tribology International, 1997, 30 (11): 807-813 28. Deng Jianxin etal. Wear resistance of Al2O3/TiB2 ceramic cutting tools in sliding wear tests and in machining processes. Journal of Materials Processing Technology, 1997, 72: 249-255 29. Deng Jianxin etal. Effect of whisker oritenation on the friction and wear behaviour of Al2O3/ TiB2/SiCw composite both in sliding wear and in cutting processes. Wear, 1996 Vol 201: 178-185 30. Deng Jianxin etal. Friction and wear behaviour of Al2O3/TiB2 ceramic composite against cemented carbide in various atmosphere at elevated temperature. Wear, 1996 Vol 195: 128-132 31. 鄧建新等. Al2O3/TiC/CaF2自潤滑陶瓷刀具切削過程中的減摩機(jī)理. 機(jī)械工程學(xué)報(bào), 2006, 42 (7): 109-113 32. 鄧建新等. 高溫自潤滑陶瓷刀具材料及其切削性能的研究. 機(jī)械工程學(xué)報(bào), 2003, 39 (8): 106-109 33. 鄧建新等. 陶瓷刀具切削加工時(shí)的磨損與潤滑及其與加工對(duì)象的匹配研究. 機(jī)械工程學(xué)報(bào), 2002, 38 (4): 40-45 主要獲獎(jiǎng) (1) 新型陶瓷噴嘴的研制開發(fā)及其沖蝕磨損機(jī)理研究,2004年獲教育部科技進(jìn)步一等獎(jiǎng)。(第1位) (2) 基于切削可靠性的陶瓷刀具材料的設(shè)計(jì)與開發(fā)研究,2002年獲山東省自然科學(xué)二等獎(jiǎng)。(第1位) (3) 高性能長壽命陶瓷噴嘴關(guān)鍵技術(shù)的研究及其應(yīng)用,2006年獲山東省技術(shù)發(fā)明二等獎(jiǎng)。(第1位) (4) 硼化鈦增強(qiáng)陶瓷刀具材料及其摩擦磨損行為研究,1998年獲山東省科技進(jìn)步二等獎(jiǎng)。(第1位) 獲專利情況 1. 發(fā)明專利:一種自潤滑陶瓷刀具材料,專利號(hào):ZL 200410024226.1 (第1位) 2. 發(fā)明專利:一種多環(huán)槽陶瓷加工工具,專利號(hào):ZL 200410035790.3 (第1位) 3. 發(fā)明專利:一種陶瓷噴砂嘴制備工藝,專利號(hào) ZL 02 1 35599.1 (第1位) 4. 發(fā)明專利:一種梯度陶瓷水煤漿噴嘴制備工藝,專利號(hào):ZL 200510042269.7 (第1位)